| Property | Value |
|---|---|
| Mechanical Properties | |
| Ultimate tensile strength | 520 – 560 MPa |
| Yield strength | 460 – 470 MPa |
| Elongation at break | 6 – 9 % |
| Thermal Properties | |
| Thermal conductivity | 130 W/(m⋅°C) |
| Post Treatments | |
| Anodizing compatibility | Not recommended – due to the high amount of zinc that the material contains, dark spots or corroded marks may be observed |
| Common Applications | |
| Fuse parts | Structural components |